Laser-melted cobalt-chrome frameworks being measured
Material

Milled and laser-melted cobalt-chrome (CoCr)

Crown and bridge frameworks, telescopic and conical work, implant bars, implant superstructures and cast partial denture frameworks in cobalt-chrome, 5-axis milled or laser-melted. At a glance: which alloy is approved for which indication.

In short: DD Bio CW from Dental Direkt is milled and approved for crowns and bridges of any span, primary and secondary components, telescopic and conical crowns, implant bars and implant superstructures. In the selective laser melting (SLM) process, we use Starbond Easy Powder from Scheftner and Mediloy S-Co from BEGO; Mediloy S-Co is additionally approved for cast partial denture frameworks and bars. Production runs on our own lines, separate from titanium and zirconia.

Which alloy for which use?

Select the planned case to see which alloy the manufacturer approves for it. “No manufacturer statement” means the instructions for use do not explicitly name that application.

Crown and bridge up to 3 units

Framework for veneering

First choice

DD Bio CWStarbond Easy PowderMediloy S-Co

Long-span bridge

from 4 units

First choice

DD Bio CWMediloy S-Co

Also suitable

Starbond Easy Powder

Telescopic and conical work

Primary and secondary components

First choice

DD Bio CW

Also suitable

Starbond Easy Powder

No manufacturer statement: Mediloy S-Co

Implant bar

on implants

First choice

DD Bio CWMediloy S-Co

No manufacturer statement: Starbond Easy Powder

Implant superstructure

screw-retained or cemented

First choice

DD Bio CW

Also suitable

Mediloy S-Co

No manufacturer statement: Starbond Easy Powder

Cast partial denture framework

Clasp and combination prosthetics

First choice

Mediloy S-Co

Also suitable

Starbond Easy Powder

No manufacturer statement: DD Bio CW

Inlay and onlay

metal

First choice

DD Bio CW

No manufacturer statement: Starbond Easy Powder, Mediloy S-Co

Laser-melted cobalt-chrome implant bar on the build platform
Cobalt-chrome in the selective laser melting (SLM) process

The alloys in detail

Bright blue means manufacturer-approved, light blue means approved with limitations, and pale means the instructions for use do not provide for that application. The bar shows the yield strength according to the manufacturer (scale up to 1200 MPa).

DD Bio CW

milledType 4Modulus of elasticity 250 GPa

Milled CoCr alloy from Dental Direkt: crowns and bridges of any span, telescopic and conical crowns, implant bars and implant superstructures.

  • Crown and bridge up to 3 unitsFirst choice
  • Long-span bridgeFirst choice
  • Telescopic and conical workFirst choice
  • Implant barFirst choice
  • Implant superstructureFirst choice
  • Cast partial denture frameworkNo manufacturer statement
  • Inlay and onlayFirst choice

Starbond Easy Powder

SLMType 5Modulus of elasticity 225 GPa

CoCr powder from Scheftner for selective laser melting: fixed and removable dental prostheses, veneered with ceramic or resin.

  • Crown and bridge up to 3 unitsFirst choice
  • Long-span bridgeSuitable
  • Telescopic and conical workSuitable
  • Implant barNo manufacturer statement
  • Implant superstructureNo manufacturer statement
  • Cast partial denture frameworkSuitable
  • Inlay and onlayNo manufacturer statement

Mediloy S-Co

SLMType 5Modulus of elasticity 228 GPa

CoCr powder from BEGO for selective laser melting: crowns, bridges, cast partial denture frameworks, bars and secondary bars, including screw-retained implant work.

  • Crown and bridge up to 3 unitsFirst choice
  • Long-span bridgeFirst choice
  • Telescopic and conical workNo manufacturer statement
  • Implant barFirst choice
  • Implant superstructureSuitable
  • Cast partial denture frameworkFirst choice
  • Inlay and onlayNo manufacturer statement

Not for: ceramic firing on abutments and screw-retained implant bridges

Strength comparison

Laser-melted alloys achieve a higher yield strength than milled DD Bio CW. The milling alloy is softer, easier to finish and explicitly approved for telescopic and conical work.

  1. DD Bio CW
    400 MPa
  2. Starbond Easy Powder
    760 MPa
  3. Mediloy S-Co
    1000 MPa

Yield strength (Rp0.2) according to the manufacturer’s instructions for use; for Mediloy S-Co, the lighter area is between the value after ceramic firing (755 MPa) and after stress-relief annealing (1000 MPa). Minimum wall thicknesses and connector cross-sections are given in the instructions for use.

Datasheets and instructions for use

Instructions for use, safety data sheet and, where available, declaration of conformity and evidence of biocompatibility. Tap the name to open.

DD Bio CWmilled CoCr, Dental Direkt

Type 4 to ISO 22674, modulus of elasticity 250 GPa, hardness 285 HV10, CTE 14.4, yield strength 400 MPa, tensile strength 680 MPa. Can be veneered with ceramic or resin; oxidation firing is not mandatory.

Starbond Easy PowderCoCr in the selective laser melting process, Scheftner

Type 5 to ISO 22674, nickel-free and beryllium-free, modulus of elasticity 225 GPa, hardness 425 HV10, CTE 14.5, yield strength 760 MPa. Stress-relief firing from 4 units; the instructions for use refer generally to fixed and removable dental prostheses.

Mediloy S-CoCoCr in the selective laser melting process, BEGO

Type 5 to ISO 22674, modulus of elasticity 228 GPa, hardness 470 HV10, CTE 14.0, yield strength 1000 MPa after stress-relief annealing (755 MPa after ceramic firing).

How your order works

Files or model

STL, PLY or OBJ via the upload portal, for example from exocad or 3Shape. Or send the model by UPS collection; we scan and design in Cologne.

Specify material

Material and, where needed, shade in the order form. If nothing is specified, we suggest the appropriate material based on the indication.

Check and production

We check wall thicknesses and connectors against the manufacturer’s specifications and call if anything is unclear before production starts.

Shipping

Files received by 14:00 count as day 1 of production; standard cases are shipped on day 2, via UPS from Cologne. All times under production times.

Other materials

Each material has its own page with indications and all datasheets:

Frequently asked questions about cobalt-chrome

Milling or laser melting: which is better?

Both have their place. Milled DD Bio CW is approved for telescopic and conical crowns, implant bars and implant superstructures. Laser-melted alloys are stronger and suitable for frameworks, cast partial denture frameworks and larger constructions. If nothing is specified, we choose the appropriate process based on the indication.

Which CoCr alloys does CADmill use?

DD Bio CW from Dental Direkt for milling, plus Starbond Easy Powder from Scheftner and Mediloy S-Co from BEGO in the selective laser melting process. Instructions for use and safety data sheets are available on this page.

Can I veneer CoCr frameworks with ceramic?

Yes, with a veneering ceramic whose CTE matches the alloy. The values are given in the instructions for use. For Mediloy S-Co, ceramic firing on abutments and screw-retained implant bridges is not approved.

What if there is a CoCr intolerance?

In that case, titanium is the alternative; see the Titanium page. If an allergy is suspected, the manufacturers recommend an allergy test in advance.

Scroll to Top